MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Afrormosia Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Tends to darken on exposure, stains in contact with iron in damp conditions.
Usual surface texture: Medium/fine
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Very Durable (Over 25 years)
Resistance to penetration by preservatives: Extremely resistant
Common Applications: Interior and exterior joinery. Furniture. Cladding.

Key Words: Pericopsis elata; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.610 g/ccGreen, African Origin
Density 0.634 g/ccat nominal specific gravity
 0.700 g/ccat oven-dry state
 0.744 g/ccNominal; at 12.0% m.c.
 0.665 - 0.867 g/ccat 12.0% m.c.
Moisture Absorption at Equilibrium 3.0 - 6.5 %Between 40% RH and 90% RH
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 6900 NSide Hardness, 12% Moisture, African Origin
 7100 NSide Hardness, Green, African Origin
Modulus of Rupture 0.102 GPaStatic Bending, Green, African Origin
 0.1269 GPaStatic Bending, 12% Moisture, African Origin
Flexural Modulus 12200 MPaStatic Bending, Green, African Origin
 13400 MPaStatic Bending, 12% Moisture, African Origin
Compressive Strength 51.6 MPaParallel to Grain, Green, African Origin
 68.5 MPaParallel to Grain, 12% Moisture, African Origin
Machinability 50 %Medium Relative to Other Wood
Shear Strength 11.5 MPaParallel to Grain, Green, African Origin
 14.4 MPaParallel to Grain, 12% Moisture, African Origin
Work to Maximum Load 0.127 J/cm³Static Bending, 12% Moisture, African Origin
 0.135 J/cm³Static Bending, Green, African Origin
 
Thermal PropertiesOriginal ValueComments
Shrinkage 3.0 %Radial Shrinkage Green to Oven Dry, African Origin
 6.4 %Tangential Shrinkage Green to Oven Dry, African Origin
 10.7 %Volumetric Shrinkage Green to Oven Dry, African Origin
 
Descriptive Properties
ColorLight Brown Usual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abarco (Albarco) Wood
African Mahogany Wood
Alerce Wood
American Andiroba Wood
American Ash Wood

PTSM001 / 71354

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.