Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast. Availability: Latin America, North America and South America Additive: - Antiblock: 6000 ppm
- Slip: 1500 ppm
- Processing Aid: Yes
- Thermal Stabilizer: Yes
Applications: - Blown Film
- Bread Bags
- Cast Film
- Food packaging
- Packaging Films
- Paper Overwrap
- Zipper Bag
Information provided by ExxonMobil |