MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lord Adhesives Metech 2539A Silver-Silver Chloride Reference Electrode Ink
Categories: Fluid

Material Notes: Silver-silver chloride reference ink is designed for screen print application onto flexible and rigid plastic substrates. It has been developed to provide a standard reference electrode potential utilizing the silver-silver chloride couple. It is used in disposable electrochemical assays and specifically for bio-electrochemical assays i.e. bio sensors.

The ink has good rheological properties and may be used in manual and high speed automatic applications. Good adhesion is achieved through low temperature drying profiles.

Although primarily intended for use on rigid PVC and flexible substrates such as polyester and polycarbonate films, the ink may be used on rigid substrates such as conventional PCB's, glass and ceramics.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 30000 - 50000 cP
@Temperature 25.0 °C
HBT, Spindle #SC4-14 @ 10rpm
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 0.175 ohm100 square pattern alumina substrate cured at 150ºC for 45 minutes
 
Component Elements PropertiesOriginal ValueComments
Silver, Ag 72 %
 
Descriptive Properties
AdhesionVery GoodTape Test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD048 / 86056

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.