MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
ATI Allvac® 3-2.5 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: Data provided by Allvac.

Applications: Excellent cold formability, 20-50% higher tensile properties than CP titanium grades. Primarily used in aircraft hydraulic systems.

Key Words: UNS R56320; AMS 4943, 4944; MIL-T-9046, -9047. ASTM B 265, 337, 338, 348, 381, Ti-3Al-2.5V; Half 6-4; Ti-3-2.5; Allvac, an Allegheny Teledyne Company
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.48 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 256Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 278Estimated from Rockwell C value.
Hardness, Rockwell C 24
Hardness, Vickers 269Estimated from Rockwell C value.
Tensile Strength, Ultimate 690 MPa
Tensile Strength, Yield 586 MPa
@Strain 0.2 %
Elongation at Break 15 %
Reduction of Area 25 %
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 3.0 %
Carbon, C <= 0.050 %
Hydrogen, H <= 0.015 %
Iron, Fe 0.13 %
Nitrogen, N 0.010 %
Oxygen, O 0.10 %
Titanium, Ti 94 %as balance
Vanadium, V 2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® 6-2-4-2 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age
Titanium Ti-3Al-2.5V (Grade 9), alpha annealed
ATI Allvac® 6-4 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Haynes Ti-3Al-2.5V Alloy Titanium Tubing
ATI Allvac® 6-4ELI Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal

NALL44 / 14794

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.