Chamotte. Bond type: Hydraulic. Description: An alumina-silica concrete with extremely high strength and abrasion resistance. For service up to 1260°C/2300°F. May be cast, gunned or trowelled over insulating refractories to obtain a high strength hot-face protection for a good insulation back-up. Information provided by Morgan Advanced Materials |