MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt C 207 LS Putty
Categories: Polymer; Adhesive; Thermoset; Polyester, TS

Material Notes: C 207 LS putty is a blue adhesive formulated from unsaturated polyesters resin that gels and cures at room temperature by adding MEKP catalyst. It can be used to bond different fiberglass parts, as a fairing and bedding compound. Color fades to beige when mixed with MEKP catalyst.

Features And Benefits:

  • Excellent adhesion fiberglass to fiberglass
  • Efficient even if thin or thick application
  • Controlled exotherm
  • Enhanced color indicator to ensure proper catalization
  • Easy to apply by hand

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.600 - 0.750 g/cc0.0217 - 0.0271 lb/in³
Brookfield Viscosity 300000 - 450000 cP300000 - 450000 cPRVT T-E @ 10rpm
 
Processing PropertiesMetricEnglishComments
Gel Time 35.0 - 45.0 min35.0 - 45.0 mincatalyzed @ 1,5% Norox MEKP 925
Shelf Life 1.50 Month1.50 Month
 
Descriptive Properties
Thixotropic Index>6
Unanalyzed ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9013 / 231608

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.