MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American Rock Elm Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Ring-Porous Hardwood. Least easy to work with hand tools. Very good steam bending, poor planing, poor shaping. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Ulmus thomasii; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.570 g/ccOven Dry Weight/Unseasoned Volume
 44.0 lb/ft³Unseasoned*
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 4400 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 4400 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 660 psiPerpendicular to Grain*
Modulus of Rupture 0.102 GPaIn Bending
 9.50 ksiStatic Bending*
Flexural Yield Strength 55.2 MPaBending stress at proportional limit
 4600 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 10.3 GPaIn Bending
 1190 ksiStatic Bending*
Compressive Strength 4.80 MPaPerpendicular to Grain
 38.0 - 49.0 MPaParallel to Grain
 750 psiPerpendicular to Grain*
 2870 psiParallel to Grain*
 3780 psiMax Crushing Strength Parallel to Grain*
Shear Strength 1270 psiParallel to Grain*
Impact 4.1in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 11000psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 1.20 in-lb/in³Static Bending*
Work to Maximum Load 19.8 in-lb/in³Static Bending*
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.300 BTU-in/hr-ft²-°F12% Moisture Content, US origin
 1.00 BTU-in/hr-ft²-°FOven Dry, US origin
Shrinkage 4.8 %Radial, from green to oven dry, US origin
 8.1 %Tangential, from green to oven dry, US origin
 8.1 %Tangential; Unseasoned to Oven Dry*
 14.9 %Volumetric, from green to oven dry, US origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sodium Chloride, NaCl (Halite)
American Maple, Rock (Sugar Maple)
3M 7000 Series Copper Roofing Granule (Little Rock)
3M #11 Roofing Granule (Little Rock)
3M Headlap Roofing Granule (Little Rock)

PTSAR / 71301

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.