MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SACO AEI CAPXIDAN® HD Modified Ethylene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Descritption: CAPXIDAN® HD is a Modified Copolymer produced with a proprietary, specialized formulation. It is designed to be coextruded over Wood-Plastic Composite (WPC) deck boards to provide moisture, stain, wear resistance, aesthetics, durability at elevated temperatures, and unprecedented adhesion to the WPC substrate. CAPXIDAN® HD is a two-component capstock system. The CAPXIDAN® resin should be extruded together with a specific synergistic additive masterbatch in the recommended proportion of 98:2 by weight.

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature <= 30.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3050 psiASTM D638
Tensile Strength, Yield 2900 psiASTM D638
Elongation at Break 400 %ASTM D638
Tensile Modulus 30000 psi
@Temperature 23.0 °C
Young’s; ISO 178
 55000 psi
@Temperature 0.000 °C
Young’s; ISO 178
 75000 psi
@Temperature -40.0 °C
Young’s; ISO 178
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µm/m-°C
@Temperature -100 - 85.0 °C
ASTM D696
Specific Heat Capacity 1.92 J/g-°C
Vicat Softening Point 124 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO000 / 249367

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.