MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CLAL-MSX NICLAFOR® 1000 TH3 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeability, good formability, long life duration. Meets environmental concern by not containing Beryllium, Cadmium nor Titanium.

Applications:

  • Electrotechnic
  • Electromechanic
  • Electronic
  • Connectic
  • Automotive
  • Domestic appliances
  • Spectacle industry
  • Turned parts.

Information provided by CLAL-MSX

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 310 - 340310 - 340
Tensile Strength, Ultimate 950 - 1050 MPa138000 - 152000 psi
Tensile Strength, Yield >= 800 MPa
@Strain 0.2 %
>= 116000 psi
@Strain 0.2 %
Elongation at Break >= 4.0 %>= 4.0 %A50 mm
Modulus of Elasticity 120 GPa17400 ksi
Modulus of Rigidity 50.0 GPa7250 ksiTorsion
Flexural Strength 829 MPa120000 psiRigidity. Elastic bending fatigue, Longitudinal
 >= 840 MPa>= 122000 psiRigidity. Elastic bending fatigue, Transverse
Fatigue Strength 450 MPa
@# of Cycles 1.00e+7
65300 psi
@# of Cycles 1.00e+7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.00001433 ohm-cm<= 0.00001433 ohm-cmprecipitation hardened (3h)
 <= 0.00001911 ohm-cm<= 0.00001911 ohm-cmquenched
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.25 µm/m-°C
@Temperature 20.0 - 200 °C
9.583 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 53.6 W/m-K372 BTU-in/hr-ft²-°F
Melting Point 968 - 1078 °C1770 - 1972 °F
Solidus 968 °C1770 °F
Liquidus 1078 °C1972 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 82.65 - 85.95 %82.65 - 85.95 %
Iron, Fe <= 0.50 %<= 0.50 %
Lead, Pb <= 0.030 %<= 0.030 %
Manganese, Mn 0.050 - 0.30 %0.050 - 0.30 %
Nickel, Ni 8.5 - 9.5 %8.5 - 9.5 %
Phosphorus, P <= 0.020 %<= 0.020 %
Tin, Sn 5.5 - 6.5 %5.5 - 6.5 %
Zinc, Zn <= 0.50 %<= 0.50 %
 
Descriptive Properties
Bending590° bending across and in the rolling direction, longitudinal
 590° bending across and in the rolling direction, transverse

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NCLAL065 / 160096

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.