MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials RTV6428 Dark Gray General Purpose Potting/Encapsulating Compound  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depths. Typical uses: Power supply encapsulation of temperature limited assemblies. "Snap cure". Automotive.

Data provided by the manufacturer, GE Silicones.

GE Silicones became a part of Momentive Performance Materials in 2006.

Key Words: RTV Silicones; R.T.V. Silicones
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/cc
Viscosity 1300 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 62
Tensile Strength, Ultimate 3.24 MPa
Elongation at Break 60 %
Tear Strength 3.40 kN/mDie B
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 5.70e+14 ohm-cm
Dielectric Constant 3.0
@Frequency 1000 Hz
Dielectric Strength 21.0 kV/mm
@Thickness 1.91 mm
Dissipation Factor 0.0061
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 210 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.310 W/m-K
Maximum Service Temperature, Air 204 °CContinuous useful temperature.
Minimum Service Temperature, Air -60.0 °CContinuous useful temperature.
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Processing Temperature 25.0 °CCure time 4 hours.
Pot Life 4.00 min
@Temperature 25.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond MasterSil 156 Two Part, Low Viscosity Silicone
Momentive Performance Materials RTV627 Dark Gray General Purpose Potting/Encapsulating Compound
Dow 3-6751 THERMALLY CONDUCTIVE ADHESIVE, KIT
Momentive Performance Materials TSE3331 Dark Gray Thermally Conductive Potting/Encapsulating Compound
CHT Group QSil 550 QSI Quantum Silicones Silicone Potting Material

PZZGE985 / 40539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.