MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asia Technology Pioneers CAP 102 PP Nanocomposite
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description: CAP102 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.

    Advantages:
  • Good paint ability
  • Good dimensional (Heat) stability
  • Outstanding surface appearance
  • UV resistance
  • Good Scratch resistance
    Certification:
  • ISO 9001:2008
  • Iranian Nano Technology Initiative Council Certification
  • Certification from automakers
    Application:
  • Automotive Interior Parts (Dashboard Items)
  • Automotive Exterior and Interior Paint-on Parts

Information provided by Asia Technology Pioneers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D792
Melt Flow 11.6 g/10 min
@Temperature 230 °C
11.6 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 37.3 MPa5400 psiASTM D638M
Flexural Strength 43.08 MPa6248 psiASTM D790
Flexural Modulus 0.206 GPa29.9 ksiASTM D790
Izod Impact, Notched 0.382 J/cm0.716 ft-lb/inASTM D256
 
Descriptive Properties
FormPellets - Tan color
Processing MethodInjection Molding
Reinforcement AdditivesNano Particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sweet Birch Wood
Sika SikaBond® Construction Adhesive One part advanced polyurethane, elastomeric adhesive
DSM Somos® NeXt LV Grey
Carbon-Core Carbon Balsa Wood

PTATP02 / 135220

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.