MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LNP Stat-Kon® MS- HI LE Polypropylene, Stainless Steel Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Stainless Fiber, EMI

Material Notes:
  • Features: Electrically Conductive, Low Extractables, High Impact Resistance
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccMethod A; ASTM D792
Linear Mold Shrinkage 0.013 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.014 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 15.2 MPaASTM D638
Tensile Strength, Yield 21.4 MPaASTM D638
Elongation at Break 76 %ASTM D638
Elongation at Yield 7.1 %ASTM D638
Tensile Modulus 1.26 GPaASTM D638
Flexural Strength 27.6 MPaASTM D790
Flexural Modulus 1.28 GPaASTM D790
Izod Impact, Notched 0.961 J/cm
@Thickness 3.18 mm
ASTM D256
Izod Impact, Unnotched 13.3 J/cm
@Thickness 3.18 mm
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²ISO 180
Falling Dart Impact 11.0 JASTM D3763
Instrumented Impact Total Energy 9.98 JMulti-Axial Instrumented Impact Energy; ISO 6603-2
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 100 - 1.00e+6 ohmASTM D4496
 
Thermal PropertiesOriginal ValueComments
CTE, linear 99.0 µm/m-°C
@Temperature 20.0 °C
TMA; ASTM E831
CTE, linear, Transverse to Flow 120 µm/m-°C
@Temperature 20.0 °C
TMA; ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 52.8 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 227 - 246 °C
Mold Temperature 32.2 - 48.9 °C
Drying Temperature 82.2 °C
Dry Time 4 hour
Back Pressure 0.172 - 0.345 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos H02C-00 Polypropylene Homopolymer
Avient Maxxam™ FR PP 301 S Polypropylene
Celanese Celstran® PP-GF30-03 Natural PP, 30% Glass Reinforced
Flint Hills AP5206-HN Polypropylene Impact Copolymer
RTP Company EMI 161 HI  Polypropylene (PP) Shielding - Stainless Steel Fiber 10% - High Impact

PZLNP1324 / 51406

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.