MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kennametal Densalloy™ SD180
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Densalloy™ provides the unique properties required in applications ranging from therapeutic medical radiation shielding to aircraft counterbalancing. Its nominal tungsten content ranges from 89% to 97% with the balance primarily of nickel and iron. By adding alloying elements to tungsten, Densalloy™ has greater ductility and better machinability than with pure tungsten.

Densalloy is similar to machining gray cast iron because the material is highly abrasive with the chips and discontinuous. Carbide tools are used for milling, turning and drilling; however, cobalt is recommended for tapping. The use of coolant is suggested for roughing but is not required for finish cutting. Cutting speeds should be in the range of 100 to 300 SFM, and feeds should be set to maintain approximately .006" to .010" chip load. Depth of cuts for roughing can be as much as 1/8" and for finishing as much as .030".

Joining: Densalloy can be joined to itself and other materials using brazing and conventional mechanical methods. Brazing is most effectively done using nickel or copper in a reducing atmosphere. Densalloy can also be very effectively joined to itself using a sinter bond technique. Sinter bonding essentially causes diffusion of material across the joint interface resulting in an almost indiscernible joint in the finished part.

Finishes - Corrosion Resistance: Although Densalloy possesses good corrosion resistance, slight corrosion will occur in high humidity atmospheres. Various finishes can be applied to improve its corrosion resistance. This includes cadmium and nickel plating as well as acrylic and epoxy paints.

Information provided by ATI Tungsten Materials, a business unit of Allegheny Technologies Incorporated (ATI).

ATI completed the sale of its Tungsten Materials Business to Kennametal Inc. on November 4, 2013.

Key Words: Mil. T-21014, Rev. D Class 3
ASTM-B-777-87 Class 3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 17.75 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C <= 34
Tensile Strength, Ultimate >= 120000 psi
Tensile Strength, Yield >= 80000 psi
@Strain 0.2 %
Elongation at Break >= 6.0 %1 inch (2.5 cm) gauge length
 
Component Elements PropertiesOriginal ValueComments
Tungsten, W 95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Densalloy™ SD170
Kennametal Densalloy™ DENS21
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Kennametal Densalloy™ SD185
Kennametal Densalloy™ DENS25

NTUNG02 / 19487

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.