MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC XENOY™ CL100 PC+PBT (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: XENOY CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior automotive applications. ISO1043: PC+PBT-I.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Density 1.22 g/ccISO 1183
Water Absorption 0.50 %23°C/sat; ISO 62
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 14 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 96.0 MPaISO 2039-1
Tensile Strength at Break 55.0 MPa50 mm/min; ASTM D638
 56.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 55.0 MPa50 mm/min; ISO 527
 56.0 MPa50 mm/min; ASTM D638
Elongation at Break 50 %50 mm/min; ASTM D638
 50 %50 mm/min; ISO 527
Elongation at Yield 5.0 %50 mm/min; ISO 527
 5.0 %50 mm/min; ASTM D638
Tensile Modulus 2150 MPa1mm/min; ISO 527
 2200 MPa5 mm/min; ASTM D638
Flexural Yield Strength 80.0 MPa2 mm/min; ISO 178
 85.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2050 MPa1.3 mm/min, 50 mm span; ASTM D790
 2050 MPa2 mm/min; ISO 178
Izod Impact, Notched 700 J/mASTM D256
 160 J/m
@Temperature -40.0 °C
ASTM D256
 170 J/m
@Temperature -30.0 °C
ASTM D256
 600 J/m
@Temperature 0.000 °C
ASTM D256
Izod Impact, Notched (ISO) 50.0 kJ/m²80*10*4; ISO 180/1A
 20.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 45.0 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 55.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 20.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 50.0 JASTM D3763
Taber Abrasion, mg/1000 Cycles 30CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 3.3
@Frequency 1e+6 Hz
IEC 60250
 3.3
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 18.0 kV/mm
@Thickness 1.00 mm
shorttime; IEC 60243-1
Dissipation Factor 0.0020
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 90.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Thermal Conductivity 0.180 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 110 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 90.0 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 90.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 125 °CRate B/50; ISO 306
 125 °CRate B/50; ASTM D1525
 127 °CRate B/120; ISO 306
 160 °CRate A/50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
Nozzle Temperature 250 - 265 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 240 - 265 °C
Zone 3 250 - 270 °C
Melt Temperature 255 - 270 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 90.0 - 100 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10830 / 244297

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.