MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elkem (Bluestar Silicones) BLUESIL™ V-1067 B Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: BLUESIL™ V-1069 is a high strength, two component, tin catalyzed, room temperature cure silicone rubber. It is designed as a 30 Shore A, thixotropic (non-sag) rubber providing excellent physical properties and long library life. Blending of BLUESIL™ V-1069 with BLUESIL™ V-1062 or BLUESIL™ V-1065 provides a unique variety of brush-on coating blends to suit the needs of many applications in the museum, architectural restoration field, theme park and the film industries.

Applications:

  • Museum reproductions
  • On-site architectural reproductions
  • Special effects and props for the film industry
  • Robotic and animatronic skins
  • Theme park props and reproduction mold

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/cc
Viscosity 25 cP25 cPPart B, Catalyst Component
 70000 cP70000 cPMixed
 75000 cP75000 cPPart A, Base Component
Linear Mold Shrinkage  <= 0.0010 cm/cm
@Time 86400 sec
<= 0.0010 in/in
@Time 24.0 hour
 0.0030 cm/cm
@Time 25200 sec
0.0030 in/in
@Time 7.00 hour
Storage Temperature 24.0 °C75.2 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 383824 hr thick section
 3838ASTM D2240
Tensile Strength 5.34 MPa775 psiASTM D412
Elongation at Break 390 %390 %ASTM D412
Tear Strength 12.3 kN/m70.0 pliASTM D624, Die B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min
@Temperature 24.0 °C
168 hour
@Temperature 75.2 °F
50% RH
Pot Life 300 min300 min
Working Life 960 min960 min
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
ColorClear or BluePart B, Catalyst Component
 WhitePart A, Base Component
Mix Ratio100:2.5A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ V 1082 HiPro ST ~ PEX Silicone Rubber
Elkem (Bluestar Silicones) SILBIONE® LSR 60 Liquid Silicone Rubber
Elkem (Bluestar Silicones) SILBIONE® LSR 4340 FC Liquid Silicone Rubber
Elkem (Bluestar Silicones) SILBIONE® LSR 4325 Liquid Silicone Rubber
Elkem (Bluestar Silicones) CAF® 530 Silicone Rubber

PBLUST062 / 191038

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.