MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik UNIPEARL® 835-1234 Colorant
Categories: Color; Other Engineering Material; Additive/Filler for Polymer

Material Notes: UNIPEARL® colorants are patented, universal, machine dispensable pearlescent colorants for use in special effect finishes. They can be used in both clear alkyd and water-based coatings. UNIPEARL® colorants can be used either by themselves in a glaze or neutral base over a colored substrate or in combination with COLORTREND® colorants.

Dispensing at the point of sale allows for the most flexibility in color and effect. Moreover, it allows the retail store to offer an unlimited palette of luminescent finishes with a small investment in inventory.

UNIPEARL® colorants are designed for use in faux finishes, decorative coatings, wall coverings and specialty finishes. UNIPEARL® colorants are compatible with nitrocellulose lacquers, epoxy alkyd, acrylic latex, catalyzed and water-reducible urethane coatings.

Since UNIPEARL® colorants do not contain a binder, they will not form a film and must be used in a coating. Recommended starting levels are 2.5 ounces of UNIPEARL® colorant to 0.5 ounces of COLORTREND® colorant in a quart of glaze, neutral base or coating. These values are flexible and can be adjusted to achieve the desired color and effect.

UNIPEARL® colorants are made with industrial grade pearlescent pigments. These pigments consist of mica platelets treated with titanium dioxide, iron oxide or a combination of both. The plate-like shapes come from the mica and the high refractive index or pearlescence comes from the titanium dioxide.

UNIPEARL® colorants have very good lightfastness and weathering characteristics. Their performance in exterior coatings is highly dependent on the choice of coating and accompanying pigments. Coatings designed for use in exterior applications should be tested to determine if they meet the end use requirements or if they require a weather-treated grade of pearlescent pigment.

UNIPEARL® colorants can be used as low as 2% by weight and as high as 15% by weight.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.28 g/cc
Density 10.7 lb/gal
Solids Content 11 %vehicle
 30 %pigment
Volatile Organic Compounds (VOC) Content 443 g/l
Volatiles 59 %
 
Descriptive Properties
ColorantPearlescent Gold

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy
Overview of materials for Epoxy, Cast, Unreinforced
Overview of materials for Epoxy Molding Compound
NRI Thermo-Fill™ Titanium Reinforcement
LKAB Minerals MicroCarb Chalk

PHUMB375 / 81377

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.