MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond F123HV Color Keyed Thixotropic Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND F123 HV is a fast cure, high viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating single or multi-channel fiber optic connectors. Although this unique three-step color- change formulation unmixed components are light yellow, it turns light green on mixing, and changes again to a deep reddish-amber after the REQUIRED 100°C HIGH-TEMPERATURE CURE. It develops strong, tough, mechanically stable bonds to a wide variety of fiber optic and optical materials that includes most metals, ceramics, glass and many plastics. TRA-BOND F123 HV has good impact and thermal shock resistance, and yields excellent low stress, pot-and-polish connections which do not piston during cycle tests. It is also resistant to water and weathering, vapors and gases, most petroleum products, and an extended range of organic and inorganic environments. Shorter cures at higher temperatures (e.g. 2 minutes at 120°C, or 1 minute @ 150°C) are also possible. An additional post-cure of 30 minutes at 150°C is recommended when application temperatures higher than 150°C are anticipated. For masses over 1/4 gram, allow material to gel for 4 hours at 25°C followed by 100°C for 5 minutes.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccMixed
Solids Content 100 %Reactive Solids Content
Viscosity 60000 cPMixed (rv #7, 10 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87
Adhesive Bond Strength 2500 psiLap shear, alum to alum
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 400 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 63.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 175 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 120 °CUltimate Tg
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.56
Transmission, Visible 93 %6000-9000 Å
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Temperature 100 °C
Pot Life 240 min
 
Descriptive Properties
Color Green BlueMixed
 Light YellowUnmixed
 Reddish-AmberCured
Mix Ratio, parts by weight100/10Resin/Hardener
Thixotropic Index 5.91 rpm/10 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAC234 / 71162

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.