MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Starflam® PX06009 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Starflam PX06009 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding Resin

Former Eurostar product. Eurostar has been acquired by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccDAM; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 95.0 MPaDAM; ISO 527-2
Elongation at Break 3.2 %DAM; ISO 527-2
Tensile Modulus 6200 MPaDAM; ISO 527-2
Flexural Strength 160 MPaDAM; ISO 178
Flexural Modulus 6200 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI 15 - 30 secPLC 3; UL 746
 >= 120 secPLC 0; UL 746
 >= 120 secPLC 0; UL 746
 >= 120 secPLC 0; UL 746
 >= 120 secPLC 0; UL 746
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 125 °C
@Thickness 0.750 mm
UL 746
 125 °C
@Thickness 0.800 mm
UL 746
 125 °C
@Thickness 1.00 mm
UL 746
 125 °C
@Thickness 1.50 mm
UL 746
 125 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 125 °C
@Thickness 0.750 mm
UL 746
 125 °C
@Thickness 0.800 mm
UL 746
 125 °C
@Thickness 1.00 mm
UL 746
 125 °C
@Thickness 1.50 mm
UL 746
 125 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 130 °C
@Thickness 0.750 mm
UL 746
 130 °C
@Thickness 0.800 mm
UL 746
 130 °C
@Thickness 1.00 mm
UL 746
 130 °C
@Thickness 1.50 mm
UL 746
 140 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-2
@Thickness 0.750 mm
 V-2
@Thickness 0.800 mm
 V-2
@Thickness 1.00 mm
 V-2
@Thickness 1.50 mm
 V-2
@Thickness 3.00 mm
Glow Wire Ignition Temperature 725 °C
@Thickness 1.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 240 - 250 °CInjection
Middle Barrel Temperature 250 - 260 °CInjection
Front Barrel Temperature 250 - 270 °CInjection
Melt Temperature 250 - 270 °CInjection
Mold Temperature 50.0 - 90.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
Moisture Content 0.20 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
Agency RatingsISO, 1043 PA6 GF20 FR(30)
AppearanceNatural Color
FeaturesFlame Retardant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Extrusion Grade
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
Edinburg Plastics DOA006 PA 6/6 Flame Retardant
Bamberger Polymers Bapolene® 5062 Polypropylene, Injection Grade

PEUROSTA19 / 172033

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.