System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC VALOX™ 420HP PBT (Europe)
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
Material Notes:
30% Glass filled PBT resin, FDA Food Contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility information. Alternative grade VALOX HX420HP.
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.53
g/cc
ASTM D792
1.53
g/cc
ASTM D792
Density
1.53
g/cc
ISO 1183
Filler Content
30 %
ASTM D229
Water Absorption
0.060 %
24 hours; ASTM D570
0.26 %
23°C/sat; ISO 62
Moisture Absorption
0.0800 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0030
-
0.0070
cm/cm
SABIC method
0.0030
-
0.0050
cm/cm
@Thickness 1.50 - 3.20 mm
SABIC method
0.0030
-
0.0080
cm/cm
@Thickness 3.20 mm
SABIC method
0.0050
-
0.0080
cm/cm
@Thickness 3.20 - 4.60 mm
SABIC method
Linear Mold Shrinkage, Transverse
0.0050
-
0.010
cm/cm
SABIC method
0.0040
-
0.0060
cm/cm
@Thickness 1.50 - 3.20 mm
SABIC method
0.0050
-
0.010
cm/cm
@Thickness 3.20 mm
SABIC method
0.0060
-
0.0090
cm/cm
@Thickness 3.20 - 4.60 mm
SABIC method
Melt Flow
13
g/10 min
@Load 2.16 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
17
g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
118
ASTM D785
Tensile Strength at Break
120
MPa
5 mm/min; ASTM D638
125
MPa
5 mm/min; ISO 527
Tensile Strength, Yield
120
MPa
5 mm/min; ASTM D638
125
MPa
5 mm/min; ISO 527
Elongation at Break
2.0 %
5 mm/min; ISO 527
3.0 %
5 mm/min; ASTM D638
Elongation at Yield
2.0 %
5 mm/min; ISO 527
3.0 %
5 mm/min; ASTM D638
Tensile Modulus
9300
MPa
5 mm/min; ASTM D638
9300
MPa
1mm/min; ISO 527
Flexural Strength
189
MPa
brk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength
195
MPa
2 mm/min; ISO 178
Flexural Modulus
7580
MPa
1.3 mm/min, 50 mm span; ASTM D790
8500
MPa
2 mm/min; ISO 178
Izod Impact, Notched
85.0
J/m
ASTM D256
80.0
J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched
801
J/m
ASTM D4812
Izod Impact, Notched (ISO)
8.00
kJ/m²
80*10*4; ISO 180/1A
7.00
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
45.0
kJ/m²
80*10*4; ISO 180/1U
45.0
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched
45.0
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
45.0
kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
5.00
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
5.00
kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
8.00
J
ASTM D3763
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
3.20e+16
ohm-cm
ASTM D257
Dielectric Constant
3.7
@Frequency 1e+6 Hz
ASTM D150
3.8
@Frequency 100 Hz
ASTM D150
Dielectric Strength
18.7
kV/mm
@Thickness 3.20 mm
in air; ASTM D149
24.8
kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
Dissipation Factor
0.0020
@Frequency 100 Hz
ASTM D150
0.020
@Frequency 1e+6 Hz
ASTM D150
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
25.2
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
25.2
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow
120
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
120
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi)
217
°C
Flatw 80*10*4 sp=64mm; ISO 75/Bf
215
°C
@Thickness 6.40 mm
unannealed; ASTM D648
220
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
204
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
203
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point
215
°C
Rate B/50; ASTM D1525
215
°C
Rate B/120; ISO 306
215
°C
Rate B/50; ISO 306
223
°C
Rate A/50; ISO 306
Processing Properties
Original Value
Comments
Nozzle Temperature
245
-
260
°C
Injection Molding
Zone 1
240
-
255
°C
Zone 2
245
-
260
°C
Zone 3
250
-
265
°C
Melt Temperature
250
-
265
°C
Mold Temperature
65.0
-
90.0
°C
Drying Temperature
120
°C
Injection Molding
Dry Time
3.00
-
4.00
hour
Injection Molding
12.0
hour
Cumulative; Injection Molding
Moisture Content
0.020 %
Back Pressure
0.300
-
0.700
MPa
Shot Size
40 - 80 %
Vent Depth
0.00250
-
0.00380
cm
Screw Speed
50
-
80
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABI10258 / 243725
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.