MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont MOLYKOTE® 33 EXTREME LOW TEMPERATURE BEARING GREASE, LIGHT
Categories: Fluid; Lubricant; Lithium Gellant; Silicone Base

Material Notes: Former Dow Corning product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/cc
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 122.3 kg
Penetration P(60), 1/10 mm 320
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -73.0 °C
Dropping Point 226 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month
 
Descriptive Properties
Colorwhite
NLGI Number1
Thickening Systemlithium soap

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont MOLYKOTE® 44 HIGH TEMPERATURE BEARING GREASE, LIGHT
NuSil Lightspan™ LS-8941 Silicone, Optical Adhesive Elastomer
DuPont MOLYKOTE® 44 HIGH TEMPERATURE BEARING GREASE, MEDIUM
Phillips 66 Syndustrial® Hydraulic Fluid ISO Grade 32
Nye Lubricants 415 (SO) Synthetic Oil

PDOWCO252 / 105953

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.