MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryer

Uses: Extrusion: Cable jacket, hose/tube, profile and film and sheet

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ASTM D2240
Hardness, Shore D 43 - 49ASTM D2240
Elongation at Break 400 %ASTM D412
100% Modulus 0.0135 GPa
@Strain 100 %
ASTM D412/D638
300% Modulus 0.0316 GPa
@Strain 300 %
ASTM D412/D638
Modulus of Rigidity 0.00840 GPa
@Temperature 23.0 °C
ASTM D1053
 0.0138 GPa
@Temperature 0.000 °C
ASTM D1053
 0.0413 GPa
@Temperature -20.0 °C
ASTM D1053
 0.2138 GPa
@Temperature -40.0 °C
ASTM D1053
 0.3656 GPa
@Temperature -50.0 °C
ASTM D1053
Flexural Modulus 10990 psiASTM D790
Tear Strength 165 pliSplit; ASTM D470
 675 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 5.0CS-17, 1000 g; ASTM D3389 B
Compression Set 36 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395
 61 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
Tensile Set 20 %200% elongation; ASTM D412/D638
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 239 °FASTM D1525
Transformation Temperature -13.0 °Fby DSC
 
Processing PropertiesOriginal ValueComments
Zone 1 182 - 188 °C
Zone 2 188 - 199 °C
Zone 3 193 - 204 °C
Zone 4 199 - 210 °C
Adapter Temperature 204 - 216 °C
Die Temperature 193 - 204 °CZone 2
 199 - 210 °CZone 1
Screw Speed 15 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® 4056 TPC-ET
Arkema Kynar® 710 Polyvinylidene Fluoride Homopolymer- Injection Molding
Covestro Desmopan® 372 Thermoplastic Polyurethane
Arkema KYNAR® 9000 HD Polyvinylidene Fluoride - Injection Molding
Syensqo (Solvay Specialty Polymers) Solef® 1008 PVDF Homopolymer

PNOVEON033 / 55299

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.