MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite North America 52-70-70-VO-P Short-Glass Reinforced Diallyl Phthalate
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled; Filled/Reinforced Thermoset

Material Notes: Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.

Conforms with the requirements of ASTM D5948 Type SDG-F.

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.91 g/ccASTM D792
Apparent Bulk Density 0.750 g/cc
Water Absorption 0.25 %48 hours, 50°C. ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cmCompression Molding. ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 75.0 MPaASTM D638
Flexural Yield Strength 124 MPaASTM D790
Flexural Modulus 11.7 GPaASTM D790
Compressive Yield Strength 150 MPaASTM D695
Izod Impact, Notched 0.320 J/cmASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.5
@Frequency 1e+6 Hz
Wet
Dielectric Strength 13.8 kV/mmWet, step-by-step. ASTM D149
Dissipation Factor 0.014
@Frequency 1e+6 Hz
Wet; ASTM D150
Arc Resistance 130 secASTM D495
Comparative Tracking Index >= 600 VASTM D3638 (IEC 112)
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Maximum Service Temperature, Air 130 °CUL temperature Index, UL 746B
Deflection Temperature at 1.8 MPa (264 psi) >= 280 °CASTM D648A
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 130 °CUL 746B
UL RTI, Mechanical without Impact 130 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.60 mm
 V-0
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 180 °CMold temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PSM Industries Pacific Sintered Metals FCC-214-S High Carbon Copper Steel Powdered Metal (MPIF FC-0208-50)
Cosmic Plastics CP7318 Short Glass Fiber Filled Diallyl Phthalate Molding Compound
PSM Industries Pacific Sintered Metals FCC-200-P High Carbon Copper Steel Powdered Metal (MPIF FC-0505-40)
PSM Industries Pacific Sintered Metals FCC-214-S(HT) High Carbon Copper Steel Powdered Metal (MPIF FC-0208-80HT)
Shin-Etsu Silicones KEG-2001-70A/B Fast Curing LIMS Silicone Rubber

PROG40 / 66251

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.