MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake PVC-1070 Film & Medical Grade Vinyl Suspension
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: This is a low molecular weight film and medical grade vinyl suspension resin. PVC-1070 is designed for clear and opaque extruded sheet, bottles, and other injection and blow molding applications. Kosher approved.

Information provided by Westlake Chemical Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density >= 0.528 g/ccPPVC24
Volatiles <= 0.35 %PPVC22
Viscosity Measurement 0.67 - 0.71Inherent Viscosity; PPVC45A
 1.87Relative Viscosity
 
Descriptive Properties
ASTM Cell ClassificationGP2-16340, ASTM D1755
Hunter Lab ColorL = >95, a= <0.9, b= <2. PPVC38
K-Value57, DIN 53726
Particle Size Distribution0% retained on 40 mesh. <5% retained on 60 mesh. <35% retained on 200 mesh. <7% retained on pan.
Residual Vinyl Chloride Monomer< 1.0 ppm, PPVC27
Syntron Contamination< 50 particles/100 gms, PPVC35

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake PVC-1100 Film & Medical Grade Vinyl Suspension
Westlake PVC-1095 Film & Medical Grade Vinyl Suspension

PWESF8845 / 222917

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.