MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lucobit Lucofin® 1414-t3 Polyolefin TPO Granules, Silk Grey
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t3 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and flexibility and resistance to weathering even at low temperatures.

Applications:
• Colored roof sheeting
• Sealing sheeting
• Construction profiles

This product is provided with special halogen free fire retardants in order to pass test method 3 of European standard EN 1187.

Information provided by Lucobit AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ISO 868
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air <= -40.0 °CLow Temperature Flexural Test; EN 495-5
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 - 200 °CProfiles
 160 - 230 °CMembranes
 160 - 270 °CCoatings
Melt Temperature 160 - 220 °C
Mold Temperature 10.0 - 40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Elastamax™ XL-2155 Thermoplastic Polyolefin Elastomer (TPO (POE))
Lanxess PUROLAN® Sericin Silk Glycoprotein
Dow SiLK™ D Semiconductor Dielectric Resin
Lucobit Lucofin® 1414 Polyolefin TPO Granules, Silk Grey
Lucobit Lucofin® 1414-t1 Polyolefin TPO Granules, Silk Grey

PLUCO941 / 151007

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.