MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Scotchrap™ 50 Tape
Categories: Polymer; Tape; Thermoplastic; Vinyl (PVC)

Material Notes: 3M™ Scotchrap™ Tapes 50 and 51 are tough, polyvinyl chloride based tapes with special high tack adhesives formulated to resist corrosion of metal piping systems above and below ground, fittings and joints on all mill-coated pipe and electrical conduit systems. These tapes are: Resistant to salt water, soil acids, alkalies and salts, common chemicals, chemical vapors, and exposure to outdoor weathering and sunlight. Resistant to impact, abrasions, punctures, and tears. Tape 50 is a highly conformable, all-weather 10 mil (0.254 mm) thick tape designed for application over a wide temperature range.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption 0.30 %ASTM D570
Water Vapor Transmission 15.5 g/m²/dayASTM D3833
Thickness 10.0 milASTM D1000
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 100 %
@Temperature -12.0 °C
ASTM D1000
 200 %
@Temperature 23.0 °C
ASTM D1000
Peel Strength 1.25 pli
@Temperature 23.0 °C
Adhesion to Steel; ASTM D1000
 1.25 pli
@Temperature 23.0 °C
Adhesion to Backing; ASTM D1000
 1.875 pli
@Temperature -12.0 °C
Adhesion to Steel; ASTM D1000
 1.875 pli
@Temperature -12.0 °C
Adhesion to Backing; ASTM D1000
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown >= 12000 VASTM D1000
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °C
Minimum Service Temperature, Air -48.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= -12.0 °CApplication
 <= 65.6 °CApplication
 
Descriptive Properties
AppearanceBlackBacking
 BlackAdhesive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35176 / 169923

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.