Product Description: Butvar® B-98 is a thermoplastic, polyvinyl butyral resin which offers a unique combination of properties for coating or adhesive applications. The use or addition of polyvinyl butyral to a system imparts adhesion, toughness, and flexibility. PVB retains the clarity of the coating and offers reactive hydroxyl sites for crosslinking with thermoset systems. Application/Uses: - Binders for adhesives and structural composites
- Binders for inks and toners
- Coatings for wood, metal or plastic substrates
Information provided by Eastman |