MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Solvay Evolite™ F1050 Thermoplastic PVDF/Carbon Fiber Composite
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), with Carbon Fiber

Material Notes: Evolite™ F1050 is a high performance thermoplastic composite material specially designed for the O&G industry. EvoliteTM F1050 is a unidirectional tape combining the recognized excellent chemical and temperature resistance of Solef® PVDF with the inherent high strength performance of carbon fiber.

Features:

  • Semi crystalline PVDF thermoplastic matrix
  • Compatibility within PVDF Solef® 60512 and other Solef® grades
  • Fully impregnated unidirectional tape
  • Maximum Service Temperature of 130°C
  • Customised Fibre/Matrix translation for maximum performance
  • Ideal processing, mechanical and chemical resistance for applications in Oil & Gas
  • Recyclable
  • 5 year storage at ambient conditions

    Information provided by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 - 1.80 g/cc0.0632 - 0.0650 lb/in³ASTM D792
Water Absorption <= 0.040 %
@Time 86400 sec
<= 0.040 %
@Time 24.0 hour
ASTM D570
Thickness 250 microns9.84 milTape
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 27.0 MPa3920 psi90° tape property; EN 2597:1998
 1850 MPa268000 psi0° tape property; ASTM D3039M
 1876 MPa272100 psi0° tape property after autoclave consolidation; ASTM D3039
Tensile Modulus 100 GPa14500 ksi0° tape property; ASTM D3039M
 112 GPa16200 ksi0° tape property after autoclave consolidation; ASTM D3039
Compressive Strength 776 MPa
@Temperature -21.0 °C
113000 psi
@Temperature -5.80 °F
0° tape property after autoclave consolidation; ASTM D6641
Shear Modulus 1.47 GPa213 ksiIPSS, 45° tape property after autoclave consolidation; ASTM D3518
Shear Strength 33.0 MPa4790 psiIPSS, 45° tape property after autoclave consolidation; ASTM D3518
 49.0 MPa7110 psiILSS, 0° tape property after autoclave consolidation; ASTM D2344
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 162 °C>= 324 °FASTM D3418
Glass Transition Temp, Tg -40.0 °C-40.0 °FASTM D4065
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month
@Temperature 22.2 °C
60.0 Month
@Temperature 72.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL9B990 / 280445

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.