MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials RTV577 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the standard curing agent. DBT is suitable for most applications, however, other catalysts are available to facilitate deep section cure, faster cure and automated mixing.

Mechanical and electrical properties for 0.5 wt% DBT curing agent added, cured 7 days at 25°C and 50% relative humidity.

Key Performance Properties:

  • Variable work times and cure rates by adjusting the amount and type of curing agent
  • Room temperature cure
  • Composition free of solvents and solvent odor
  • Excellent adhesion capabilities with primer
  • Excellent release properties

Applications:

  • Cast-in-place heat shielding
  • Thermal insulation
  • Low and high-temperature bonding
  • Potting and encapsulation of electrical assemblies

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/cc
Viscosity 700000 cP
Linear Mold Shrinkage 0.0065 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 48
Tensile Strength, Ultimate 31.0 kg(f)/cm²
Elongation at Break 150 %
Tear Strength 6.80 kg(f)/cm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.60e+14 ohm-cm
Dielectric Constant 3.9
@Frequency 1000 Hz
Dielectric Strength 18.5 kV/mm
Dissipation Factor 0.020
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.350 BTU/lb-°F
Thermal Conductivity 0.310 W/m-K
Maximum Service Temperature, Air 204 °CContinuous
 260 °CIntermittent
Brittleness Temperature -115 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
@Temperature 25.0 °C
0.5% DBT curing agent added
 
Descriptive Properties
ColorWhite
ConsistencyPaste
Work Time2 hoursAt 25°C, 0.5% DBT curing agent added

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV511 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White
Momentive Performance Materials RTV5222 Neutral Cure, One Component RTV Adhesive Sealant
Momentive Performance Materials RTV560 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, Red
Momentive Performance Materials RTV566 Silicone Rubber Compound for Low Outgassing Applications
Momentive Performance Materials RTV577 White Extreme Low Temperature Potting/Encapsulating Compound

PGESIL032 / 41023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.