MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Stratasys® Vero™ VEROBLACKPLUS RGD875 PolyJet 3D Printing PhotoPolymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Vero is a Rigid Opaque photoPolymer Combination that provides excellent detail visualization and can be blended with other photoPolymer Combinations to vary hardness, flexibility, translucency or heat resistance. 3D print smooth, attractive prototypes to test the fit, form, and function of your static parts, moving components or complex assemblies. Use production systems such as the Stratasys J750 and Connex3 and their multi-material and multi-colour features to produce an impressive range of photorealistic visual effects and lifelike details.

Characteristics

  • Opaque
  • Rigid
  • Dimensionally stable
Options
  • Provide excellent detail visualization
  • 3D print accurate, attractive prototypes that test fit, form and function, even for moving and assembled parts.
  • Produce smooth, accurate jigs, fixtures and manufacturing tooling
Uses
  • Form and fit testing
  • Moving parts and assembled parts
  • Sales, marketing and exhibition models
  • Assembly of electronic components
  • Silicon molding
Advantages
  • Outstanding versatility
  • Fine detail

Information provided by Proto3000

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 - 1.18 g/cc0.0423 - 0.0426 lb/in³ASTM D792
Ash 0.0100 - 0.0200 %0.0100 - 0.0200 %USP281
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 73.0 - 76.073.0 - 76.0
Hardness, Shore D 83.0 - 86.083.0 - 86.0
Tensile Strength 50.0 - 65.0 MPa7250 - 9430 psiASTM D-638-03
Elongation at Break 10.0 - 25.0 %10.0 - 25.0 %ASTM D-638-05
Modulus of Elasticity 2.00 - 3.00 GPa290 - 435 ksiASTM D-638-04
Flexural Strength 75.0 - 110 MPa10900 - 16000 psiASTM D-790-03
Flexural Modulus 2.20 - 3.20 GPa319 - 464 ksiASTM D-790-04
Izod Impact, Notched 0.200 - 0.300 J/cm0.375 - 0.562 ft-lb/inASTM D256-06
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 - 50.0 °C113 - 122 °FASTM D648-06
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °C113 - 122 °FASTM D648-06
Glass Transition Temp, Tg 52.0 - 54.0 °C126 - 129 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPROTO828 / 322841

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.