MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik DYNACOLL® 7381 Copolyester
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: DYNACOLL® 7000 products are linear copolyesters with primary hydroxyl functionality and medium molecular weight.

Our DYNACOLL® 7000 product line is designed as a building block system, allowing the tailormade production of reactive hot melts (RHM). The 7300 series is a crystalline

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/cc
@Temperature 23.0 °C
Viscosity 2000 cP
@Temperature 80.0 °C
Molecular Weight 3500 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 2.0[mg KOH/g]
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 20.0 MPawith MDI; OH:NCO=1:2.11
Elongation at Break 80 %with MDI; OH:NCO=1:2.11
 
Thermal PropertiesOriginal ValueComments
Melting Point 65.0 °C
Softening Point 73.0 °C
Flash Point >= 300 °C
 
Descriptive Properties
Hydroxyl Number (mg KOH/g)27-34

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik DYNACOLL® 7380 Copolyester

PHUMB216 / 81218

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.