MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American Ponderosa Pine Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Softwood. Easy to work with hand tools. Data is based on small, clear, air-dried samples unless specified.

Key Words: Pinus ponderosa; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.400 g/ccAir Dry (12-15% Moisture Content)
Cell Length 3.60 mmMature Wood
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 2000 NSide
Tensile Strength, Ultimate 2.80 MPaPerpendicular to Grain
Modulus of Rupture 0.0630 GPaIn Bending
Flexural Yield Strength 43.4 MPaBending stress at proportional limit
Flexural Modulus 8.69 - 9.00 GPaIn Bending
Compressive Strength 5.10 MPaPerpendicular to Grain
 36.0 - 36.5 MPaParallel to Grain
Poissons Ratio 0.337µLR, 12% Moisture Content
 0.359µTR, 12% Moisture Content
 0.40µLT, 12% Moisture Content
 0.426µRT, 12% Moisture Content
Shear Strength 8.00 MPaOrientation Unknown
Toughness 16.9 JRadial
 21.5 JTangential
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.690 BTU-in/hr-ft²-°FOven Dry
 0.840 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 3.9 %Radial; Green to Zero Moisture
 6.3 %Tangential; Green to Zero Moisture
 9.6 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Eastern White Pine Wood
Lodgepole Pine Wood
American Pine Wood
Northern White Pine Wood
American Balsam Fir Wood

PTSAJ / 71293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.