HG385MO is a polypropylene homopolymer intended for injection molding. This grade combines unique Borstar® reactor design with Borstar® nucleation technology to produce highly-crystalline polypropylene. This product is characterized by excellent flow properties combined with a narrow molecular weight distribution well suited for low distortion products. This grade contains anti-static and slip additives, which result in short cycle time, good demolding and low dust attraction. Products molded from this grade exhibit excellent dimension consistency combined with high stiffness. Applications: caps and closures, and items requiring good antistatic properties.Information provided by Borealis AG |