MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Plexus Plexus™ MA320 Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.

Excellent low temperature and toughness properties.

Information provided by Illinois Tool Works.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 lb/galMixed
Viscosity 40000 - 60000 cPB
 135000 - 175000 cPA
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2000 - 2500 psi
Elongation at Break 100 - 140 %
Tensile Modulus 30000 - 40000 psi
Shear Strength 1500 - 2000 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -67.0 °F
Flash Point 51.0 °FTCC
 
Processing PropertiesOriginal ValueComments
Pot Life 8.0 - 12 min
 
Descriptive Properties
ColorOff-white, white, or black
Fixture Time25-30 minutes
Gap FillingMax 0.375 in
Mix Ratio10:1By volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ITW Devcon Composite Welder™ Methacrylate Adhesive FS, Blue Green, Black
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 1.75 - 2.50 in Rod or Thickness; Per ASTM F136)
TIMET TIMETAL® 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, <3.00 in, Annealed, Per ASTM B348
Titanium Ti-6Al-4V ELI (Grade 23), Annealed

PMM9002 / 53310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.