MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound OF008AE Polyphenylene Sulfide, Branched (PPS, Branched)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LNP THERMOCOMP OF008AE compound is based on branched Polyphenylene Sulfide (PPS) resin containing 40% glass fiber. Added features of this grade include: Easy Molding.

Features: High Stiffness,Easy Molding,Structural

Information provided by SABIC

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccASTM D792
Density 1.70 g/cc0.0614 lb/in³ASTM D792
Moisture Absorption 0.130 %0.130 %23°C / 50% RH; ISO 62
 0.210 %0.210 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0036 cm/cm0.0036 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 128 MPa18600 psi5 mm/min; ISO 527
 133 MPa19300 psi5 mm/min; ASTM D638
Elongation at Break 0.90 %0.90 %5 mm/min; ASTM D638
 0.90 %0.90 %5 mm/min; ISO 527
Tensile Modulus 16.34 GPa2370 ksi1 mm/min; ISO 527
 17.04 GPa2471 ksi5 mm/min; ASTM D638
Flexural Strength 197 MPa28600 psiISO 178
 205 MPa29700 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 15.45 GPa2241 ksi2 mm/min; ISO 178
 16.1 GPa2340 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 90.0 J66.4 ft-lbASTM D256
Izod Impact, Unnotched 2.97 J/cm5.56 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 18.0 kJ/m²8.57 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 4.00 J2.95 ft-lbASTM D3763
Impact Test 2.00 J1.48 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
10.6 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 37.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
20.6 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 277 °C531 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 280 °C
@Thickness 3.20 mm
536 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 266 °C511 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 271 °C
@Thickness 3.20 mm
520 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 320 - 330 °C608 - 626 °F
Zone 3 330 - 345 °C626 - 653 °F
Melt Temperature 315 - 320 °C599 - 608 °FInjection Molding
Mold Temperature 140 - 165 °C284 - 329 °F
Drying Temperature 120 - 150 °C248 - 302 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81757 / 289704

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.