MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Xencor™ HPPA LGF-4060 High Performance (HPPA), Long Glass Fiber Thermoplastic
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: Long Glass Fiber Thermoplastic. PA base, 60% LGF. Black.

Xencor™ HPPA LGF-4060 is a 60% Long Glass Fiber reinforced, easy-flowing, heat stabilized HPPA with a very high flexural modulus. It exhibits unique stiffness/toughness combination, an excellent retention of properties in a wide temperature range, as well as outstanding creep and fatigue resistance.

Xencor™ HPPA LGF-4060 has a pellet length of 9mm and can be processed on most injection-molding machines. It is available in black.

Black: Xencor™ HPPA LGF-4060 BK 000-9

Applications: Aircraft Applications; Automotive Applications; Consumer Applications; Industrial Applications

Features: Creep Resistant; Electrically Insulating; Fatigue Resistant; High Impact Resistance; High Temperature Stiffness; Hot Water Moldability; Low CLTE; Low Shrinkage; Low Warpage

Injection notes: Pre-Drying -- Since polyamides are hygroscopic materials as well as sensitive to moisture during processing, this product should always be pre-dried.
Regrind -- Regrind of highly filled thermoplastic materials, such as this material, should only be recycled with special care. The regrind content must never exceed 20% and only regrind of optimum quality should be used. In any case, part properties should be checked.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.69 g/ccISO 1183
Moisture Absorption 1.20 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPa
@Temperature 70.0 °C
ISO 527-2
 285 MPa
@Temperature 23.0 °C
ISO 527-2
Elongation at Break 2.0 %ISO 527-2
Tensile Modulus 17000 MPa
@Temperature 70.0 °C
ISO 527-2
 22500 MPa
@Temperature 23.0 °C
ISO 527-2
Flexural Strength 420 MPaISO 178
Flexural Modulus 21500 MPaISO 178
Charpy Impact Unnotched 100 kJ/m²
@Temperature -30.0 °C
ISO 179
 110 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 60.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 60.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+13 ohmASTM D257
Dielectric Strength 35.0 kV/mm
@Thickness 2.00 mm
IEC 60243-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 18.0 µm/m-°CISO 11359-2
Thermal Conductivity 0.350 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 260 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 255 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 290 - 300 °C
Middle Barrel Temperature 300 °C
Front Barrel Temperature 300 °C
Nozzle Temperature 300 °C
Melt Temperature <= 320 °CInjection
Mold Temperature 80.0 - 120 °C
Drying Temperature 80.0 °C
@Time 14400 - 28800 sec
Moisture Content <= 0.10 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingCompression Molding; Injection Molding; Overmolding
RoHS ComplianceYes
Suggested Max Regrind (%)20Injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4621 / 280421

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.