MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Blue River Coatings High Performance Acrylic Topcoat
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC TOPCOAT is a water dispersible acrylic enamel. HIGH PERFORMANCE ACRYLIC TOPCOAT is designed to be a low VOC and EPA compliant coating with excellent coverage and mar resistance. HIGH PERFORMANCE ACRYLIC is an ideal topcoat to replace solvent base acrylic enamel.

Enviromental Advantages:BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC TOPCOAT is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated, dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling.

Characteristics:

  • Good exterior durability
  • Available in satin to gloss finish
  • Good hardness/impact resistance
  • Water is used for reduction
  • Excellent performance on most plastics
  • Water is used for clean-up
  • Non-Hazardous
  • Air dry or force curing preferred
  • Wide range of colors
  • Coating will not flash rust on bare metal
  • Shelf life of 1 year
  • Unused paint can be returned to container
  • Non-Flammable
  • Uses

  • Fiberglass
  • Steel
  • Aluminum
  • Plastic
  • Wood
  • PVC
  • Information provided by Blue River Coatings

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity >= 1.00 g/cc
    Density 8.70 lb/gal
    Solids Content 39.2 %by volume
     43 %by weight
    Volatile Organic Compounds (VOC) Content 144 g/l
     
    Thermal PropertiesOriginal ValueComments
    Boiling Point 169 °C
    Flash Point 150 °F
     
    Processing PropertiesOriginal ValueComments
    Cure Time 0.167 hour
    @Temperature 75.0 °C
    Recoat, at 50% humidity
     0.330 hour
    @Temperature 75.0 °C
    Dust Free, at 50% humidity
     0.750 hour
    @Temperature 75.0 °C
    Dry to handle, at 50% humidity and 75°C
    Shelf Life 12.0 Month
     
    Descriptive Properties
    FlexibilityGood
    Pencil HardnessHB
    Salt SprayGood
    Solvent ResistanceGood; 20 double rubs
    Theoretical Coverage628 ft2 at 1 mil

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    WBLUER07 / 74606

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.