System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Omya OMYAFLOW® F - SY Calcium Carbonate
Categories:
Ceramic
;
Other Engineering Material
;
Additive/Filler for Polymer
Material Notes:
A high purity, fine, wet ground natural calcium carbonate available in slurry form.
Applications
: Decorative paints.
Information supplied by Omya North America.
Key Words:
CaCO3
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.88
g/cc
Density
15.66
lb/gal
Slurry
Solids Content
74 %
as Supplied
Brightness
96 %
Y - Brightness (dry)
Particle Size
1.4
µm
Median Diameter
Specific Surface Area
7.0
m²/g
Brookfield Viscosity
200
cP
@Temperature 25.0 °C
No. 3 Spindle, 100 rpm
Compliance Properties
Original Value
Comments
FDA
Yes
21 CFR 174.5, 175.300, 178.3297
Descriptive Properties
Calcium Carbonate %
98
Magnesium Carbonate %
1
Percent Finer than 1 Microns
40
Percent Finer than 2 Microns
60
Pounds Pigment/gallon (slurry)
11.59
Pounds Pigment/Solid Gallon (dry)
11.59
Retained in 325 mesh (dry) ppm
2
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Omya OMYAFLOW® UF - SY Calcium Carbonate
Omya OMYAFLOW® 3 - SY Calcium Carbonate
Omya OMYACARB® 6 - PT Calcium Carbonate
Omya OMYACARB® 4 - LU Calcium Carbonate
Omya OMYACARB® 5 - FL Calcium Carbonate
EOMYA939 / 5651
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.