MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayflex® WR-20 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Characterization: Bayflex WR-20 is a solid elastomer which has a flexural modulus of 3,000 psi (21 MPa)* at room temperature.

Properties / Applications: Bayflex WR-20 is a solid elastomer which has a flexural modulus of 3,000 psi (21 MPa)* at room temperature. It is processed on reaction injection molding (RIM) equipment and is used for rollers, gaskets, and encapsulated windows. This system combines rapid demold times, excellent integrity at demold, improved release characteristics, and outstanding physical properties.The Bayflex WR-20 system was developed to add a weather-resistant grade to our range of window encapsulation systems. In some cases, the weatherability of this system eliminates the need for post-painting or in-mold coatings. This product is available only in black. Bayflex WR-20 is a formulated RIM system supplied as two reactive liquid components. Component A is a diphenylmethane diisocyanate (MDI) prepolymer, and Component B is a polyether polyol. As with any product, use of the Bayflex WR-20 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccPolyol (Component B)
 1.21 g/ccIsocyanate (Component A)
Density 1.10 g/ccASTM D1622
Water Absorption 3.8 %
@Time 86400 sec
Bayer
 7.4 %
@Time 864000 sec
Bayer
Viscosity 700 cPIsocyanate (Component A)
 1400 cPPolyol (Component B)
Linear Mold Shrinkage 0.014 cm/cmBayer Test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70ASTM D2240
Tensile Strength, Ultimate 11.0 MPaASTM D412
Elongation at Break 450 %ASTM D412
Flexural Modulus 0.0170 GPa
@Temperature 65.0 °C
ASTM D790
 0.0210 GPa
@Temperature 23.0 °C
ASTM D790
 0.0610 GPa
@Temperature -30.0 °C
ASTM D790
Tear Strength 33.0 kN/mDie C; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Flash Point 191 °CPolyol (Component B)
 213 °CIsocyanate (Component A)
 
Processing PropertiesOriginal ValueComments
Mold Temperature 60.0 - 70.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® XGT-140 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® 110-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Covestro Bayflex® XGT-16 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)

PB2B85 / 26627

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.