MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Molding M6162  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, High Impact; PVC, Rigid Grade

Material Notes: Custom Molding

This compound is in natural color and is not suitable for outdoor applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmASTM D955
Spiral Flow 58.4 cmRelative Spiral Flow; 23
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 79
@Time 10.0 sec
ASTM D2240
Tensile Strength, Yield 46.2 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 50 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2240 MPaType I, 51 mm/min; ASTM D638
Flexural Strength 68.3 MPaASTM D790
Flexural Modulus 2280 MPaASTM D790
Izod Impact, Notched 133 J/m
@Thickness 3.18 mm,
Temperature -18.0 °C
Injection Molded; ASTM D256A
 641 J/m
@Thickness 3.18 mm,
Temperature 0.000 °C
Injection Molded; ASTM D256A
 961 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
Dart Drop Total Energy 89.0 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
Procedure A, 1/8-in. conical; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 140 µm/m-°CASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 77.3 °C
@Thickness 3.18 mm
Unannealed, Injection Molded; ASTM D648
 82.0 °C
@Thickness 3.18 mm
Injection Molded; Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.4 °C
@Thickness 3.18 mm
Unannealed, Injection Molded; ASTM D648
 74.1 °C
@Thickness 3.18 mm
Injection Molded; Annealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 210 °C
 
Descriptive Properties
AppearanceOpaque
FeaturesGeneral Purpose
 High Impact Resistance
 Medium Flow
FormsPellets
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConstruction Applications
 General Purpose

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PH1PN8868 / 102704

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.