MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Master Bond EP77M-1 Fast Setting, Silver Conductive Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Polymer System EP77M-1 is a two component, silver filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated temperatures. It readily develops a high bonding strength of more than 2000 psi tensile shear when measured and cured at 75°F. It is 100% reactive and does not contain any diluents or solvents. The volume resistivity of the cured system is less than 10-3 ohm-cm. EP77M-1 offers superior dimensional stability. Master Bond Polymer System EP77M-1 can be applied with minimal sagging or dripping even on vertical surfaces although it can be made thinner (flowable) by adding 5 to 10% of an appropriate solvent (xylene, acetone, MEK, etc.) by weight. The high strength bonds are remarkably resistant to chemicals including water, oil and most organic solvents, over the exceptionally wide temperature range of -60 to +300°F. Adhesion to metals, glass, ceramics, vulcanized rubbers and many plastics is excellent. Part A is silver, Part B is a clear liquid. Master Bond EP77M-1 adhesive is widely used in the electronic, electrical, computer, semiconductor, microwave, appliance, and automotive industries, among others. For convenient handling, EP77M-1 is now available in premixed and frozen syringes.

Product Advantages:

  • Contains no volatiles; excellent low outgassing properties
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures as required
  • High electrical conductivity
  • High bond strength to similar and dissimilar substrates
  • Superior durability, thermal shock and chemical resistance
  • Good rigidity and dimensional stability.
  • Widely used in military and piezoceramic applications.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Shear Strength >= 13.27 MPa>= 1925 psiBond, After 30 days water immersion, Al to Al
 >= 13.8 MPa>= 2000 psiBond, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0010 ohm-cm<= 0.0010 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.59 W/m-K11.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1080 - 1440 min18.0 - 24.0 hour85% of maximum strength developed
Pot Life 45 - 60 min45 - 60 min100 gram batch
Shelf Life 3.00 Month3.00 Monthin syringe
 6.00 Month6.00 Monthin glass jar
 
Descriptive Properties
Mixing Ratio (A to B)100/08by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Cyclo Olefin Polymer
Lehvoss LUVOCOM® 1-8864/ES Polyamide 66 with steel fiber
Lehvoss LUVOCOM® 1850-8023 PBT with carbon fiber
Lehvoss LUVOCOM® 16-8960/ES Polyarylamide with carbon fiber and steel fiber
E-Glass Fiber, Generic

PMASTB414 / 149661

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.