MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling Glastic SG-200 Corner Angles
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Corner angles used for coil winding.

Information provided by Glastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.85 g/ccASTM D-792
Water Absorption 0.15 %% by wt.; ASTM D-570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 70000 psiASTM D-638
Tensile Modulus 3.00e+6 psiASTM D-638
Flexural Strength 80000 psiASTM D-790
Flexural Modulus 3.90e+6 psiASTM D-790
Compressive Strength 14000 psiTransverse; ASTM D-695
 50000 psiAxial; ASTM D-695
Shear Strength 3000 psiIn plane; ASTM D-3914
Izod Impact, Notched 40.0 ft-lb/inASTM D-256
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 6.40e+15 ohmASTM D-257
Dielectric Constant 5.0
@Frequency 60 Hz
ASTM D-150
Dielectric Strength 2.80 kV/mm1" Axial in Oil; ASTM D-149
Arc Resistance 150 secASTM D-495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.00 µm/m-°C
@Temperature 20.0 °C
ASTM D-696
Thermal Conductivity 0.290 W/m-KASTM C-177
Flammability, UL94 HB
 
Descriptive Properties
Standard ColorTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 60% Glass Fiber Filled
ChevronTexaco Texmar 16 SG SAE 30
Borealis Daplen™ KB4436 TPO Compound
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
Magnesium ZC71-T6

PGLASW3 / 41937

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.