MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Platilon® 2102 A Polyurethane (Ester) Film
Categories: Polymer; Film

Material Notes: Product Description: PlatilonU is the trade name for extruded thermoplastic polyurethane (TPU) films made by Epurex Films. The range currently includes aromatic TPU based on polyester and polyether.

Properties: PlatilonU films are noted for the following properties:

  • high abrasion resistance
  • flexibility over a wide temperature range
  • high resistance to oils, greases and solvents
  • good weathering resistance
  • good microbial and hydrolysis resistance of polyether TPU
  • good resistance to high-energy radiation
  • free of plasticisers
  • breathable: watertight, but high water vapour transmission rate
  • good adhesion to foams, adhesives, inks and many substratesApplications: The wide range of properties of PlatilonU films is used in many different applications, such as the following:
    • Automotive: for the production of various interior trim parts e.g. headliners, door panels, seats, parcel shelves, sound insulation parts
    • Building & Construction: roof linings, pipe relining
    • Medical: colostomy bags, inflatable mattresses, antidecubitus mattresses, wound dressings, extra corporal breast prosthesis
    • Industrial: tank liners, air ducting, conveyor belts etc.
    • Sports and Leisure: sportswear, football outer skins and bladders, air cushions of athletic shoes etc.

    Information provided by Covestro

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 1.21 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore A 93ASTM D2240
    Tensile Strength at Break 70.0 MPaDIN EN ISO 527
    Tensile Stress at Strain 6.00 - 9.00 MPa
    @Strain 50 %
    DIN EN ISO 527
    Elongation at Break 450 %DIN EN ISO 527
    Tear Strength 75.0 kN/mDIN ISO 34-1, B
     
    Thermal PropertiesOriginal ValueComments
    Softening Point 150 - 175 °CTMA Onset

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Overview of materials for Silicone Polyurethane, Ether Based
    Covestro DUREFLEX® U073 TPU
    Covestro Platilon® 4100 D Polyurethane (Ester) Film
    Covestro DUREFLEX® PS5400 TPU
    Covestro DUREFLEX® X2103 TPU

    PCOVEST0967 / 202750

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.