MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Schott MICROCROWN Glass for Microscopy Slides
Categories: Ceramic; Glass; Optical

Material Notes: MICROCROWN up-drawn crown glass has one of the lowest iron contents known in the market today. It has a high luminous transmittance and an excellent colorless appearance. MICROCROWN is available as sheet glass in a thickness of 1.0 mm. Its unique composition makes MICROCROWN the right choice for microscopic slides where low auto- fluorescence and excellent chemical resistance are required.

Applications: Microscopic slides

  • High transmittance
  • Colorless appearance
  • Good cosmetic quality
  • Easy to cut by scribe and break
  • Excellent flatness
  • Resistant to chemical attack
  • Low auto-fluorescence
  • Good wettability on both glass surfaces

    Information provided by SCHOTT.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 2.55 g/cc
    Thickness 100 microns
     
    Electrical PropertiesOriginal ValueComments
    Dielectric Constant 7.0
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 9.40 µm/m-°C
    @Temperature 20.0 - 300 °C
    Transformation Temperature, Tg 533 °C
     
    Optical PropertiesOriginal ValueComments
    Refractive Index 1.522
    Transmission, Visible 97.8 %D65

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    CSGT9944 / 183197

    Proto3000 – 3D Engineering Solutions

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.