MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2125 Rigid Syntactic Repair Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-BOND 2125 is a medium viscosity, low density syntactic foam epoxy formulation developed for industrial, electronic and aerospace honeycomb, fillet, edge-fill, contour repair, bonding and casting applications where a light-weight, low shrinkage and low expansion material is required. This adhesive is color-coded for smooth, easy mixing and handling at room temperature, and it develops strong, highly reliable bonds to most surfaces including metals, building construction products, glass and glass fabrics and many plastics. TRA- BOND 2125 is a completely unicellular material composed of micron-sized glass spheres in a high performance epoxy binder, has a very uniform point-to-point structure and exhibits low shrinkage during cure, good dimensional stability, low density, high strength-to-weight ratio, high dielectric strength, and a low dielectric constant. The fully cured adhesive is a strong, light weight and durable electrical insulator which can be cut, drilled, sawed and shaped as needed with ordinary shop tools. In addition, TRA-BOND 2125 is resistant to water, weather, gases and vapors, salt and salt solutions, mild acids and alkalis, alcohol, jet fuels, gasoline and other petroleum products, and many other organic and inorganic compounds.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.800 g/ccMixed
Viscosity 35000 cP
@Temperature 25.0 °C
After mixing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75
Compressive Strength 13000 psi
Izod Impact, Notched 0.200 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.40e+15 ohm-cm
Dielectric Constant 2.9
@Frequency 1000 Hz
Dielectric Strength 375 V/mil
Dissipation Factor 0.010
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.130 W/m-K
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 hour4 hrs @ 25°C + 4 hrs @ 65°C
 24.0 hour
@Temperature 25.0 °C
Pot Life 45 min
 
Descriptive Properties
Color Light Gray
Mix Ratio, parts by weight100/9Resin/Hardener
Outgassing, NASA Passes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond K6 Ablative Thermal Epoxy Compound
Henkel Hysol EA 9396.6MD Paste Adhesive System
CMT Materials HYTAC® W Low Thermal Conductivity Epoxy Syntactic
Abatron AboCast 8504-1 One-Component Epoxy

PTRAC021 / 70949

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.