MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Fibre Glast 2443 Kevlar® Twill Weave Fabric
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Aramid

Material Notes: This Kevlar® fabric provides the improved cosmetics and drapability of a twill weave. Ideal for impact resistant applications requiring the lightweight, high strength properties of Kevlar® where pattern show-through is desirable.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Weave Pattern2x2 twill
Weight (oz/sq yd)5.3
Yarn Description, Fill1140 Denier Kevlar® 49
Yarn Description, Warp1140 Denier Kevlar® 49

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fibre Glast 549 Kevlar® Fabric
DuPont™ Kevlar® 29 Aramid Fiber
Hexcel® HexForce™ 328 Aramid Fabric
DuPont™ Kevlar® 49 Aramid Fiber
DuPont™ Kevlar® Aramid Pulp

PFIBRE111 / 104548

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.