MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Potters Industries Ballotini® Impact Beads
Categories: Ceramic; Glass

Material Notes: Ballotini® impact beads are microspheres are used for precise metal finishing of parts. They offer an environmentally safe and cost effective method for metal surface cleaning and finishing.

Coarse Beads

  • Remove larger, tougher soils.
  • Peen to more intense levels.
  • Peen to deeper zones in surface.
  • Produce higher surface profile.
  • Produce brighter surface.

Fine Beads

  • Remove smaller, lighter soil.
  • Yield more impacts per pound.
  • Clean faster.
  • Peen to less intense levels.
  • Peen outer zones of surfaces.
  • Reach into keyways, fillets, and small areas.
  • Produce lower surface profile.
  • Produce matte finish.

Information provided by Potters Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.45 - 2.50 g/cc
Density 2.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 515
Compressive Strength 36000 psiaverage
 
Descriptive Properties
Colorclear
Free Silica Content (%)0
Shapespherical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 2218-T61 (Includes Creep/Rupture/Fatigue Data)
Aluminum 1100-H18
AISI 8640H Steel, quenched 845°C (1550°F), 650°C (1200°F) temper
Potters Industries A100 Solid Glass Spheres
Aluminum 6069-T6, Hot Impact Extruded Cylinder, Minimum Tensile Values

CPOT9901 / 161891

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.