MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Osprey CE7 Al-Si Controlled Expansion Alloy
Categories: Metal; Nonferrous Metal

Material Notes: Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.

Information provided to MatWeb by Osprey Metals, now Sandvik Osprey Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 255
Tensile Strength, Ultimate 100 MPa
Modulus of Elasticity 125 GPa
Flexural Strength 143 MPaThree Point Bend
Poissons Ratio 0.25
Fracture Toughness 6.00 MPa-m½
Shear Modulus 50.0 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.70 µm/m-°C
@Temperature 25.0 - 500 °C
 7.80 µm/m-°C
@Temperature 25.0 - 100 °C
 8.30 µm/m-°C
@Temperature 25.0 - 200 °C
 8.50 µm/m-°C
@Temperature 25.0 - 300 °C
Specific Heat Capacity 0.750 J/g-°C
Thermal Conductivity 100 W/m-K
@Temperature 200 °C
 120 W/m-K
@Temperature 25.0 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 30 %
Silicon, Si 70 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Osprey CE11 Al-Si Controlled Expansion Alloy
Sandvik Osprey CE13 Al-Si Controlled Expansion Alloy
Sandvik Osprey CE17 Al-Si Controlled Expansion Alloy
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
Schott P-SF8 Glass

NOSPRCE5 / 18714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.