MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Maxxam™ FR PO Conc 62 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.

MAXXAM FR PO Concentrate 62 is designated to impart good flame retardancy and UV stbility to low and high density polyethylene. Because there are so many varieties of polyethylene, it is difficult to predict the let-down ratio required to meet the specific flammability standards. For starting point formulations we would suggest:4-7 parts by weight of Low Density Polyethylene-,5 parts by weight of High Density Polyethylene-to 1 part of Concentrate 62. When this concentrate is letdown at the proper ratio the resulting materials can achieve flame retardancy equivalent to the requirements of the UL-94 V-2 or VTM-2. BFD IX-1 and NFPA 701 preformance criteria achievable using 8% PO CONC 62 in LDPE film @ 4-8 mil film / V-2 preformance criteria achievable in PE @ 15-30% in thickness >/= 1.5mm. The effects on the physicals should be minimal.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.67 g/ccASTM D792
Melt Flow 2.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Procedure A; ASTM D1238
 
Descriptive Properties
FeaturesFlame Retardant
FormsPellets
Generic MaterialPP, Unspecified
Generic NamePolypropylene, Unspecified (PP, Unspecified)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Maxxam™ FR PP 307 Polypropylene
Avient Maxxam™ FR PP 301 S Polypropylene
Avient Maxxam™ FR PP 301 EXT Polypropylene
Avient Maxxam™ FR PP FR 8-6 A NATURAL - ROHS Polypropylene
Avient Maxxam™ FR PE CONC 1 Polyethylene, Low Density (LDPE)

PH0POL0718 / 145287

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.