Stamylex 1026F is an octene based linear low density polyethylene produced in a solution polymerization process using a Ziegler-Natta catalyst. CAS-No. 26221-73-8 Special Features: - High puncture resistance
- Very good optical properties
- Excellent sealability, in particular high hot-tack
Applications: - Pallet stretch wrap
- Form-fill-and-seal films
- Coextruded films for general packaging purposes, but in particular food packaging lamination films
- Diaper films
Information provided by Borealis AG |