MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wellman PP A422-LG60 Polypropylene with 60% Long Glass Fiber
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 60% Glass Fiber Filler

Material Notes: Long Glass Fiber Reinforced PP (LFT) produced by a pultrusion process. The pellet length is 10-15mm. PRET LFT provides outstanding mechanical performance and dimensional stability. Other benefits include high impact resistance, heat resistance, low warpage, low odor, and low VOC.

Features: Combination of high level of stiffness, strength, and toughness, Weight reduction, Dimensional stability, Corrosion resistance, Heat resistance.

Applications: Instrument Panel, Front End Module, Door Panel, Mirror Bracket, Floor Console.

Information provided by Wellman Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccISO 1183
Filler Content 60 %Glass; ISO 3451
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cmPRET
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 125 MPa5mm/min; ISO 527
Elongation at Break 1.0 %5mm/min; ISO 527
Tensile Modulus 17000 MPa1 mm/min; ISO 527
Flexural Strength 190 MPa2mm/min; ISO 178
Flexural Modulus 16000 MPa2mm/min; ISO 178
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature 23.0 °C
ISO 178
Charpy Impact, Notched 25.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 162 °CISO 75
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 230 - 250 °C
Middle Barrel Temperature 240 - 260 °C
Front Barrel Temperature 250 - 270 °C
Nozzle Temperature 250 - 270 °C
Melt Temperature 250 - 280 °C
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 90.0 - 110 °C
@Time 7200 - 14400 sec
Moisture Content <= 0.20 %
Injection Pressure 40.0 - 130 MPa
Back Pressure 0.100 - 0.500 MPa
Screw Speed 20 - 70 rpm
 
Descriptive Properties
Injection Speedslow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWEL00912 / 250034

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.